PETG is PLA's tougher, grumpier older sibling. eSUN's version has fans, a few stringing complaints, and a price that won't make you wince.
PETG is what many makers move to when PLA is not tough enough, such as brackets, garden bits and parts that sit in a warm car. eSUN's version is listed with a recommended nozzle range of 230–250°C and a heated bed at 75–90°C, which means your printer needs to run noticeably hotter than for PLA.
Our verdict: a good second material to keep on the shelf. Skip it if you only print decoration.
Pros
- More heat tolerant and tougher than PLA, generally
- Described as having a tight diameter tolerance (no figure given)
- Vacuum sealed with desiccant
- Rated 4.6 out of 5 from 74 ratings on one retailer's page
Cons
- Needs higher nozzle and bed temperatures than PLA
- Stringing is a common PETG complaint, and one 4-star buyer reported it here
- One buyer reported a strong smell while printing
- Absorbs moisture, so storage matters
What the internet says
A summary of public reviews, forum threads and owner feedback we read, as of 17 November 2026. These are other people's opinions, linked at the bottom.
What people love
- Good flow with no blobs or clogs, according to buyer ratings
- Sticks well to the bed
- Rated 4.6 out of 5 from 74 ratings on one retailer's page
What people complain about
- Stringing, a common PETG complaint, was reported by a buyer
- One buyer reported a strong smell while printing
- Often needs temperature tuning below the stated range
The consensus: Well liked for the money, as long as you are happy to tune PETG a little.
See today's price for the eSUN PETG (1.75 mm, 1 kg) on Amazon → (affiliate link)
What buyers say
On the retailer page we read, the 5-star reviews mention good flow with no blobs or clogs and good bed adhesion. One said that lowering the temperature to about 200°C, below the stated range, greatly reduced stringing and improved quality. A 4-star review reported some stringing and a strong smell.
Our take
Treat the stated temperature range as a starting point and expect to tune. If stringing appears, dry the spool before blaming the printer.
Who it isn't for
- Anyone who wants a fuss-free first spool
- People printing in poorly ventilated spaces who are sensitive to smells
Specifications
| Diameter | 1.75 mm |
|---|---|
| Net filament | 1 kg |
| Recommended print temperature | 230–250 °C |
| Recommended bed temperature | 75–90 °C |
Manufacturer figures. We have not bench-tested these.
Alternatives
- Polymaker PolyLite PLAeasier to print, less heat tolerant
- Creality Space Pi V2for drying PETG
Questions
Is PETG better than PLA?
It is tougher and more heat tolerant, but harder to print cleanly. Choose by what the part has to survive.
Does PETG need drying?
It absorbs moisture, and damp spools cause stringing and bubbling. A dryer or sealed storage helps.
What we read
This is a research review. We have not tested the product ourselves. Our opinions are based on these sources: